+ | ABS have more shrinkage than PLA. If you have thick corner on your model, the material have internal force to warp. There are some technic to solve this problem: | ||
+ | 1) Changing to PLA is the easiest way to solve this problem. | ||
+ | |||
+ | 2) Add a thin extension pad around the corner can increase stickiness to the platform. | ||
+ | |||
+ | 3) Reduce thickness of corner, ex: add hole on thick wall. | ||
+ | |||
+ | 4) Reduce distance between nozzle and platform, heat platform to 85C degree. To increase stickiness. | ||
+ | |||
+ | Reference for advance user: [[can_i_increase_heat_bed_output_watt|Increase heat bed output power]] |